Composition | Y2O3(10 mol%)-ZrO2(90 mol%) |
---|---|
Crystal system | Cubic |
Crystal structure | CaF2 |
Lattice constant | a=0.5139 nm |
Melting point | 2500 ℃ |
Density | 6.05 g/cm3(20 ℃) |
Dielectric constant | 27 |
Thermal expansion coefficient | 10.3×10-6/℃ |
Transmittance of YSZ
Size (Outer size tolerance: ±0.1 mm / Thickness tolerance: ±0.05 mm) |
10×10×0.5 t 15×15×0.5 t |
---|---|
Orientation (Tolerance: ±0.5°) |
(100), (111) |
Polishing | One-side / Both-side |
Surface roughness | Ra≦1.0 nm, Rmax≦5.0 nm |
Options | OFF substrate Breakable substrate |